View Single Post
Old 07-28-2009, 05:45 AM   #9 (permalink)
bdkw1

Senior Member
 
bdkw1's Avatar
 
Join Date: Jul 2006
Location: So Cal
Posts: 2,149



Default Re: Sheet metal formed trailing arms - WHAT THICKNESS

I would also suggest wrapping the outer bushing/hiem housing. They have a nasty habit of ripping out.

The bottoms will see the most abuse and should be thicker, like 8 gauge. 12 gauge is fine for the sides and top. Internal ribs can be 14 gauge. And yes, you need them.
bdkw1 is offline   Reply With Quote